Opis izdelkov
|
Tehnični standard
|
EN10147, EN10142, DIN 17162, JIS G3302, ASTM A653
|
|||
|
Jeklena ocena
|
DX51D, DX52D, DX53D, DX54D, S220GD, S250GD, S280GD, S350GD, S350GD, S550GD; SGCC, SGHC, SGCH, SGH340, SGH400, SGH440, SGH490,
SGH540, SGCD1, SGCD2, SGCD3, SGC340, SGC340, SGC490, SGC570; SQ CR22 (230), SQ CR22 (255), SQ CR40 (275), SQ CR50 (340), SQ CR80 (550), CQ, FS, DDS, EDDS, SQ CR33 (230), SQ CR37 (255), SQCR40 (275), SQ CR50 (340), SQ CR80 (550); ali zahteve stranke |
|||
|
Tip
|
Pocinkana tuljava
|
|||
|
Debelina
|
0. 12-6. 00 mm ali zahteva kupca
|
|||
|
Širina
|
600mm -1500 mm, v skladu z zahtevo stranke
|
|||
|
Vrsta prevleke
|
Cink
|
|||
|
Cinkova prevleka
|
30-275g/m2
|
|||
|
Površinsko obdelavo
|
Pasivacija (c), olje (o), lak za tesnjenje (L), fosfatiranje (p), neobdelano (U)
|
|||
|
Površinska struktura
|
Običajni premaz (NS), minimalizirana premaza za spangle (MS), brez sponka (FS)
|
|||
|
Kakovost
|
Odobril SGS, ISO
|
|||
|
Paket
|
Izvozi standardni paket, paket ali potreben.
|
|||
|
Izvozni trg
|
Evropa, Afrika, Srednja Azija, jugovzhodna Azija, Bližnji vzhod, Južna Amerika, Severna Amerika itd.
|
|||

Aplikacija izdelka
Galvanizirani proizvodi tuljave se uporabljajo predvsem v gradbeništvu, lahkih industriji, avtomobilih, kmetijstvu, živalih, ribolovu in gospodarskih industrijah. Gradbena industrija se uporablja predvsem za proizvodnjo korozijskih industrijskih in civilnih stavbnih plošč, strešnih žarov itd. Svetlobna industrija jo uporablja za izdelavo školjk za domače aparate, civilne dimnike, kuhinjske pripomočke itd.
naprave itd. Travna reklama, ki se uporablja predvsem kot shranjevanje in prevoz materialov, orodja za embalažo in tako naprej.