Dom-znanje-

Vsebine

Katalog izdelkov iz hladno valjane pocinkane pločevine

May 22, 2024

Katalog izdelkov iz hladno valjane pocinkane pločevine
Ime izdelka Specifikacija Razred izdelka Izvedbeni standardi Uporaba
Debelina, mm Širina, mm
Hladno vroče pocinkan jekleni trak za hladno preoblikovanje

0.4-2.5

1000-1500

DX51D+Z

Q/TB 305-2017;2012JX18;

Splošna uporaba

EN10346:2015;

EN10346:2015/JT012-2016

0.4-2.5

1000-1500

DC51D+Z

Q/TB 305-2017

0.4-2.5

1000-1500

CS A

ASTM A653/A653M:2001;ASTM A653/A653M:2001/2011JX10;2016JX059

0.4-2.5

1000-1500

CS A (Dodaj B)

dogovor

0.4-2.5

1000-1500

CS B

ASTM A653/A653M:2001;ASTM A653/A653M:2001/2011JX10;ASTM A653:2001;2016JX057;2016JX059

0.4-2.5

1000-1500

CS B (Dodaj B)

dogovor

0.4-2.5

1000-1500

G01

MS 2385:2011

0.4-2.5

1000-1500

SGCC

JIS G 3302:2010

0.4-2.5

1000-1500

2016JX006

   

Q/TB 304-2017

0.4-2.5

1000-1500

SGCC (Dodaj B)

dogovor

0.4-2.5

1000-1500

FS A

ASTM A653/A653M:2001

0.4-2.5

1000-1500

FS B

ASTM A653/A653M:2001

0.4-2.5

1000-1500

DX53D+Z

EN 10346:2015

Za globoko vlečenje
Hladno vroče pocinkan jekleni trak za splošne konstrukcije

0.4-2.0

1000-1500

S250GD+Z

GB/T 2518-2008

Za običajno strukturo

EN 10346:2015

Q/TB 305-2017

0.4-2.0

1000-1500

S280GD+Z

GB/T 2518-2008

EN 10346:2015

Q/TB 305-2017

0.4-2.0

1000-1500

S320GD+Z

GB/T 2518-2008

EN 10346:2015

Q/TB 305-2017

0.4-2.0

1000-1500

S350GD+Z

GB/T 2518-2008

EN 10346:2015

Q/TB 305-2017

0.4-2.0

1000-1500

S390GD+Z

EN 10346:2015

Q/TB 305-2017

0.5-2.0

1000-1500

S420GD+Z

EN 10346:2015

Q/TB 305-2017

0.5-2.0

1000-1500

S450GD+Z

EN 10346:2015

Q/TB 305-2017

0.4-2.0

1000-1500

S550GD+Z

GB/T 2518-2008

EN 10346:2015

Q/TB 305-2017

0.4-2.0

1000-1500

SS230

ASTM A653/A653M:2001

0.4-2.0

1000-1500

SS255

ASTM A653/A653M:2001

0.4-2.0

1000-1500

SS275

ASTM A653/A653M:2001

0.4-2.0

1000-1500

SS275 (Dodaj B)

dogovor

0.4-2.0

1000-1500

SS340

ASTM A653/A653M:2001

0.4-2.0

1000-1500

SS340 (Dodaj B)

dogovor

0.4-2.0

1000-1500

SS380

ASTM A653/A653M:2009

0.4-2.0

1000-1500

SS450

dogovor

0.4-2.0

1000-1500

SS550

ASTM A653/A653M:2001

0.4-2.0

1000-1500

SGC340

JIS G 3302-1998

Q/TB 304-2015

0.4-2.0

1000-1500

SGC400

JIS G 3302-1998

Q/TB 304-2015

0.4-2.0

1000-1500

SGC440

JIS G 3302-1998

Q/TB 304-2017

0.4-2.0

1000-1500

SGC490

JIS G 3302-1998

Q/TB 304-2017

0.4-2.0

1000-1500

SGC550

JIS G 3302-1998

Q/TB 304-2017

0.4-2.0

1000-1500

C350

KOT 1163-2009

0.4-2.0

1000-1500

C450

KOT 1163-2009

0.4-2.0

1000-1500

G350

KOT 1397-2001

0.4-2.0

1000-1500

G450

KOT 1397-2001

0.4-2.0

1000-1500

G550

KOT 1397-2001

Vroče vroče pocinkan jekleni trak za hladno preoblikovanje

1.8-4.0

900-1524

DX51D+Z

GB/T 2518-2008

Splošna uporaba

EN 10346:2015

Q/TB 305-2017

1.8-4.0

900-1524

DD51D+Z

GB/T 2518-2008

Q/TB 305-2017

1.8-4.0

900-1524

CS A

ASTM A653/A653M:2001

1.8-4.0

900-1524

CS B

ASTM A653/A653M:2001

1.8-4.0

900-1524

CS A (Dodaj B)

dogovor

1.8-4.0

900-1524

CS B (Dodaj B)

dogovor

1.8-4.0

1219-1250

G01

MS 2385:2011

1.8-4.0

900-1524

SGHC

JIS G 3302-1998

Q/TB 304-2017

1.8-4.0

900-1524

SGHC (dodaj B)

dogovor
Toplotna podlaga iz vroče pocinkanega jeklenega traku za splošno konstrukcijo

1.8-4.0

900-1500

S250GD+Z

GB/T 2518-2008

Za običajno strukturo

EN 10346:2015

Q/TB 305-2017

1.8-4.0

900-1500

S280GD+Z

GB/T 2518-2008

EN 10346:2015

Q/TB 305-2017

1.8-4.0

900-1500

S320GD+Z

GB/T 2518-2008

EN 10346:2015

Q/TB 305-2017

1.8-4.0

900-1500

S350GD+Z

GB/T 2518-2008

EN 10346:2015

Q/TB 305-2017

1.8-4.0

900-1500

S390GD+ZS420GD+Z

EN 10346:2015

Q/TB 305-2017

EN 10346:2015

1.8-4.0

1000-1500

S450GD+Z

Q/TB 305-2017

EN 10346:2015

1.8-4.0

900-1500

SS230

Q/TB 305-2017

ASTM A653/A653M:2001

1.8-4.0

900-1500

SS275

ASTM A653/A653M:2001

ASTM A653/A653M:2001

1.8-4.0

900-1500

SS275 (加B)

dogovor

1.8-4.0

900-1500

SS340

ASTM A653/A653M:2001

1.8-4.0

900-1500

SS340 (加B)

dogovor

1.8-4.0

900-1500

SGH340

JIS G 3302-1998

1.8-4.0

900-1500

SGH400

JIS G 3302-1998

1.8-4.0

900-1500

SGH440

Q/TB 304-2017

JIS G 3302-1998

1.8-4.0

900-1500

SGH490

Q/TB 304-2017

JIS G 3302-1998

1.8-4.0

900-1500

CA350

Q/TB 304-2017

dogovor

1.8-4.0

900-1500

C450

KOT 1163-2009

1.8-4.0

900-1500

G350

KOT 1397-2001

1.8-4.0

900-1500

G450

KOT 1397-2001

Cink aluminij magnezij

0.4-2.5

900-1500

DX51D+ZM/DC51D+ZM

EN 10346:2015 JT005-2018Tangshan Iron and Steel Tehnični pogoji

Splošna uporaba

0.4-2.5

900-1500

DC52D+ZM

EN 10346:2015 JT005-2018Tangshan Iron and Steel Tehnični pogoji

Za žigosanje

0.4-2.5

900-1500

DX53D+ZM

EN 10346:2015 Tehnični pogoji JT005-2018Tangshan Iron and Steel

0.4-2.5

900-1500

DC53D+ZM

EN 10346:2015 JT005-2018Tangshan Iron and Steel Tehnični pogoji

 

0.4-2.5

900-1500

S220GD+ZM

EN 10346:2015 JT005-2018Tangshan Iron and Steel Tehnični pogoji

Za običajno strukturo

0.4-2.5

900-1500

S250GD+ZM

EN 10346:2015 JT005-2018Tangshan Iron and Steel Tehnični pogoji

0.4-2.5

900-1500

S280GD+ZM

EN 10346:2015 JT005-2018Tangshan Iron and Steel Tehnični pogoji

0.4-2.5

900-1500

S320GD+ZM

EN 10346:2015 JT005-2018Tangshan Iron and Steel Tehnični pogoji

0.4-2.5

900-1500

S350GD+ZM

EN 10346:2015 JT005-2018Tangshan Iron and Steel Tehnični pogoji

0.4-2.5

900-1500

S390GD+ZM

EN 10346:2015 JT005-2018Tangshan Iron and Steel Tehnični pogoji

0.4-2.5

900-1500

S420GD+ZM

EN 10346:2015 JT005-2018Tangshan Iron and Steel Tehnični pogoji

0.4-2.5

900-1500

S450GD+ZM

EN 10346:2015 JT005-2018Tangshan Iron and Steel Tehnični pogoji

0.4-2.5

900-1500

S550GD+ZM

EN 10346:2015 JT005-2018Tangshan Iron and Steel Tehnični pogoji

0.4-2.3

900-1500

S390GD+AZ /SS410

GB/T2518-XXXX EN 10346:2015 ASTM A 792/A 792M-09

   
metal sheet aluzinc
Velika bleščeča pocinkana pločevina
galvanized coating
Pocinkana pločevina

kontaktiraj nas

Pišite nam zdaj, da dobite ponudbo izdelka!

E-naslov:gi@gneesteel.com
Whatsapp/Wechat:+8615824687445

Pošlji povpraševanje

Pošlji povpraševanje